Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 89.4 °C | 193 °F | ASTM D1525 |
I. Stern 550 High Impact Polystyrene Features:Good process propertiesExcellent toughness and environmental stress crackingApplicationsStructural foamDisplaysSmall appliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Informat.. |
|||
Vicat Softening Point | >= 89.5 °C | >= 193 °F | ASTM D1525 |
Iran Petrochemical (PCC) GPPS 1540 Polystyrene GPPS 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impa.. |
|||
Vicat Softening Point | 89.4 °C | 193 °F | 120°C.hr, 9.8N; ASTM D1525 |
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |