Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 189 °C | 372 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I.. |
|||
Vicat Softening Point | 189 °C | 372 °F | B |
Plastcom SLOVAMID 6 MI PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |