Thermal Properties Metric English Comments
Vicat Softening Point 63.9 °C
147 °F
ASTM D1525
ExxonMobil OPTEMA™ TC 115 Blown Film Resin  (discontinued **)
OPTEMA TC 115 is an ethylene methyl acrylate copolymer, designed for specialty blown film applications. It yields soft, elastic films.Information provided by ExxonMobil Chemical
Vicat Softening Point 64.0 °C
147 °F
ASTM D1525
DuPont Bynel® E403 Acid-Modified Ethylene Terpolymer Adhesive Resin  (discontinued **)
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Vicat Softening Point 64.0 °C
147 °F
ASTM D1525
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin  (discontinued **)
Appeel 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including poly..
Vicat Softening Point 64.0 °C
147 °F
1000g; ASTM D-1525
ExxonMobil Escorene® LD-720 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength p..
Vicat Softening Point 64.0 - 178 °C
147 - 352 °F
Average value: 117 °C Grade Count:9
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Vicat Softening Point 64.0 °C
147 °F
ASTM D1525
DuPont™ Surlyn® 1605SBR Sodium Ionomer Resin for Extrusion Coating  (discontinued **)
Surlyn® 1605SBR is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceuti..
Vicat Softening Point 64.0 °C
147 °F
ISO 306
Iran Petrochemical (PCC) I2 HB 7250 High Density Polyethylene
I2 (HB 7250) is a high density polyethylene with Propylene as comonomer. It is easy flowing, low warpage, less hard and stiff than I1.Applications: household articles, closures/seals, packaging.Info..
Vicat Softening Point 64.0 °C
147 °F
50°C/h; 50N; 10x10x4mm; ISO 306/B50
SYNTHOS Krasten® FB28 High Impact Polystyrene And Polyethylene Blend
Polymer blend HIPS/PE. High toughness, very good tensile properties and environmental stress cracking resistance. Processed mainly by extrusion and thermoforming. Production of sheets and films, tec..
Vicat Softening Point 64.0 °C
147 °F
ASTM D1525
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Vicat Softening Point 64.0 °C
147 °F
ISO 306
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch..
Vicat Softening Point 64.0 °C
147 °F
ASTM D1525
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Vicat Softening Point 64.0 °C
147 °F
VST/A50; ISO 306
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC)
TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be..
Vicat Softening Point 63.9 °C
147 °F
ASTM D1525
ExxonMobil Escorene® LD 713.93 Cast Film Resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin..
Vicat Softening Point 64.0 °C
147 °F
ASTM D1525
DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces..
Vicat Softening Point 64.0 °C
147 °F
BASF Novolen® 2309 L Polypropylene
Cast film and thermoformed partsData was collected by ISO methods and provided by BASF.
Vicat Softening Point 63.9 °C
147 °F
ASTM D1525
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin
Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A..
Vicat Softening Point 64.0 °C

@Load 1.02 kg
147 °F

@Load 2.25 lb
ASTM D1525
Arkema Group LOTRYL® 16 MA 003 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 16 MA 003 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 16 MA 003 is a polymer o..
Copyright © lookpolymers.com All Rights Reserved