Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 57.0 °C | 135 °F | Vicat A, 1 kg; DIN 53460/ISO 306 |
Advanced Elastomer Systems VistaFlex® 911-N Thermoplastic Rubber
(discontinued **) Description: A colorable high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as fr.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | ASTM D1525 |
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | ASTM D1525 |
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-722 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 8610 Sodium Ionomer
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low melt index sodium ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact stre.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | VST/A/50; ISO 306 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | |
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D1525 |
ExxonMobil Escor™ 5200 Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5200 is an ethylene acrylic acid copolymer with a high comonomer content. Escore 5200 can be used pure or as a component in blend formulations for bonding applications whe.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | Rate B, ASTM D1525-70 |
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D882 |
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D1525 |
Dow AMPLIFY™ EA 101 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 101 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | |
BASF Novolen® 2500 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | |
Biomer P209 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D882 |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |
|||
Vicat Softening Point | 57.0 °C | 135 °F | A50; ISO 306 |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade) Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible.. |