Polymer Property : Vicat Softening Point = 133 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 56.0 °C

@Load 1.00 kg
133 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding
Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.Main Applications: Green..
Vicat Softening Point 56.0 °C
133 °F
ISO 306/B50
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b..
Vicat Softening Point 56.0 - 145 °C
133 - 293 °F
Average value: 92.1 °C Grade Count:68
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Vicat Softening Point 56.0 - 58.0 °C

@Load 5.00 kg
133 - 136 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RE 265/D Rigid PVC, Extrusion
Semi-rigid furniture border
Vicat Softening Point 56.0 °C
133 °F
B120; ISO 306
Inno-Comp INNOPOL® CS 2-2000 TO Polypropylene Block-Copolymer Based Compound
INNOPOL® CS 2-2000 TO is a polypropylene block-copolymer based compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-2000 TO is developed for producing injection m..
Vicat Softening Point 56.1 °C
133 °F
A50 (50°C/h 10 N); ISO 306
LyondellBasell Hifaxâ„¢ A Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA 10 A is a thermoplastic polyolefin which has been developed for the extrusion and calendering of soft film and sheet. Thanks to its high rubber content "Hifax" CA 10 A fe..
Vicat Softening Point 56.0 °C
133 °F
(50 °C/h / 50N) - B/50; ISO 306
Styrolution Styrolux 3G33 SBC
Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and ..
Vicat Softening Point 56.0 °C
133 °F
B (50N); ISO 306
Borealis Daplen™ ED206HP TPO Compound
Daplen ED206HP is a 25% mineral reinforced compound intended for injection molding. ED206HP has been developed especially for the car industry, to be used in interior parts requiring excellent scra..
Vicat Softening Point 56.0 °C
133 °F
B (50N); ISO 306
Borealis Daplen™ KSR65T20 Polypropylene Compound 20% Mineral Filled
Daplen KSR65T20 is a 20% mineral filled grade for injection molding. Daplen KSR65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSR65T20 offers very g..
Vicat Softening Point 56.0 °C
133 °F
ASTM D1525
Westlake EMAC® SP2258 17% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2258 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s..
Vicat Softening Point 56.0 °C
133 °F
A50; DIN 53460
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 56.0 °C
133 °F
ASTM D1525
DuPont Bynel® 3861 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Vicat Softening Point 56.0 °C
133 °F
A50; DIN 53460
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 56.0 °C
133 °F
A50; DIN 53460
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 56.0 °C
133 °F
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical
Vicat Softening Point 56.1 °C
133 °F
ASTM D1525
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications
Product Description: Exact 4056 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin can be used in blends with polyolefins to improve..
Vicat Softening Point 56.0 °C
133 °F
ASTM D1525 and ISO 306/A
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin
Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Vicat Softening Point 56.0 °C
133 °F
ASTM D1525
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Vicat Softening Point 56.0 °C
133 °F
B50 (50N); ISO 306
Domo 2600PC Polypropylene Copolymer
Information provided by Domo.
Vicat Softening Point 56.1 °C
133 °F
ASTM D1525
Dow AMPLIFY™ EA 102 Ethylene-ethyl Acrylate (EEA)
AMPLIFY™ EA 102 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer..
Vicat Softening Point 56.0 °C
133 °F
ASTM D1525, ISO 306
DuPont™ Elvaloy® AC 2618 Ethylene Methyl Acrylate
Elvaloy® AC 2618 is a copolymer of ethylene and ethyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC..
Vicat Softening Point 56.0 °C
133 °F
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
Vicat Softening Point 56.0 °C
133 °F
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
Vicat Softening Point 56.0 °C
133 °F
BASF Procom® D 1195 Polypropylene
Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 56.0 - 79.0 °C
133 - 174 °F
Average value: 70.1 °C Grade Count:27
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..