Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 127 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 23.0 - 127 °C
73.4 - 261 °F
Average value: 64.9 °C Grade Count:66
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Vicat Softening Point 95.0 - 127 °C
203 - 261 °F
ASTM D1525
Micropol Microlink XL Crosslinkable Polyethylene
Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi..
Vicat Softening Point 114 - 127 °C
237 - 261 °F
Average value: 119 °C Grade Count:4
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..