Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.464 GPa @Temperature 200 °C |
67.3 ksi @Temperature 392 °F |
DAM; ISO 6721 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |