Polymer Property : Shear Modulus = 0.628 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.628 GPa

@Temperature 110 °C
91.1 ksi

@Temperature 230 °F
DAM; ISO 6721
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Shear Modulus 0.628 GPa

@Temperature 60.0 °C
91.1 ksi

@Temperature 140 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500AF Acetal (POM)  (Unverified Data**)
20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi..
Shear Modulus 0.628 GPa

@Temperature 70.0 °C
91.1 ksi

@Temperature 158 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Shear Modulus 0.628 GPa

@Temperature 70.0 °C
91.1 ksi

@Temperature 158 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..