Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 68.9 MPa @Temperature 121 °C |
9990 psi @Temperature 250 °F |
Short Beam, Dry |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Shear Strength | 68.9 MPa @Temperature 82.0 °C |
9990 psi @Temperature 180 °F |
Short Beam, Wet |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Shear Strength | 68.9 MPa @Temperature 232 °C |
9990 psi @Temperature 450 °F |
Short Beam; 804 Hrs |
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 68.9 MPa @Temperature 232 °C |
9990 psi @Temperature 450 °F |
Short Beam; Autoclave Cured; [0°]16 |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |