Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 66.0 MPa @Temperature 232 °C |
9570 psi @Temperature 450 °F |
Short Beam; 1255 Hrs |
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 66.0 MPa @Temperature 23.0 °C |
9570 psi @Temperature 73.4 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon Fiber Designation: C280T4; Twill 4x4Information provided by HexCel |
|||
Shear Strength | 66.0 MPa @Temperature 23.0 °C |
9570 psi @Temperature 73.4 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |