Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 47.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 47.6 MPa

@Temperature 23.9 °C
6900 psi

@Temperature 75.0 °F
Short-Beam, Dry, Autoclave; ASTM D2344
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Shear Strength 47.6 MPa

@Temperature 82.2 °C
6900 psi

@Temperature 180 °F
Beam, V-Notched; Wet; Autoclave Cured; ASTM D5379-93
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 6K 4HS IM7 Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 47.6 MPa

@Temperature 22.8 °C
6900 psi

@Temperature 73.0 °F
Laminate property; In Plane Shear; Conditioning: Dry
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l..
Shear Strength 47.6 MPa

@Temperature 93.3 °C
6900 psi

@Temperature 200 °F
0° Short Beam, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber
Information provided by HexCel