Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.76 MPa @Temperature 177 °C |
400 psi @Temperature 351 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% .. |
|||
Shear Strength | 2.76 MPa @Temperature 177 °C |
400 psi @Temperature 351 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Shear Strength | 2.76 MPa @Temperature 82.0 °C |
400 psi @Temperature 180 °F |
Overlap |
3M Scotch-Weld™ EC2216 Structural Adhesive High Performance, Very flexible bondsInformation provided by 3M |
|||
Shear Strength | 2.76 MPa @Temperature 177 °C |
400 psi @Temperature 351 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°.. |