Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 25.4 MPa @Temperature 23.9 °C |
3690 psi @Temperature 75.0 °F |
(+7 days water soak), with Arovex Carbon Fiber Epoxy Laminate |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods.. |
|||
Shear Strength | 25.4 MPa @Temperature 25.0 °C |
3690 psi @Temperature 77.0 °F |
Tensile, Al/Al lap joint; cured 2 hours @ 93°C |
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |