Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 24.8 MPa @Temperature 23.9 °C |
3600 psi @Temperature 75.0 °F |
Cure cycle: 7 days @ RT (+7 days water soak) , with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Shear Strength | 24.8 MPa @Temperature 204 °C |
3600 psi @Temperature 400 °F |
Tensile Lap Shear; Aluminum No Primer; ASTM D1002 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Shear Strength | 24.8 MPa @Temperature 21.1 °C |
3600 psi @Temperature 70.0 °F |
Tensile Lap Shear; Titanium with HP655P; ASTM D1002 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |
|||
Shear Strength | 24.8 MPa @Temperature 121 °C |
3600 psi @Temperature 250 °F |
Overlap |
3M Scotch-Weld™ 1469 One-Part Epoxy Adhesives and Metal Primer High Temperature strength and Low ViscosityInformation provided by 3M |
|||
Shear Strength | 24.8 MPa @Temperature 71.0 °C |
3600 psi @Temperature 160 °F |
with Scotch-Weld EW-5000, 14 days at 71°C and 95% RH; ASTM D1002-10 |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |
|||
Shear Strength | 24.8 MPa @Temperature 82.0 °C |
3600 psi @Temperature 180 °F |
Adhered: 50 MIL (17-7 Stainless Steel), Adhesive AF-126 (0.06 wt) |
3M Scotch-Weld™ 3901 Metal Primer 3M™ Scotch-Weld™ Metal Primer 3901 is a primer for 3M™ Scotch-Weld™ film and liquid adhesives in those applications where it is desired to obtain improved metal and glass adhesion or improved re.. |