Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 18.9 MPa @Temperature 23.9 °C |
2740 psi @Temperature 75.0 °F |
Tensile lap, Al/Al |
Master Bond EP126 Two Component Toughened Epoxy Adhesive System Master Bond Polymer System EP126 is a two component toughened epoxy resin based high temperature resistant adhesive system with continuous service capability at 500°F and outstanding chemical resis.. |
|||
Shear Strength | 18.9 MPa @Temperature -55.0 °C |
2740 psi @Temperature -67.0 °F |
Tube Shear; Dry; 60 min @ 120°C; EN2667-2 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |