Mechanical Properties Metric English Comments
Shear Strength 17.9 MPa

@Temperature 204 °C
2600 psi

@Temperature 400 °F
Short Beam; Dry; ASTM D2344
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Shear Strength 17.9 MPa

@Temperature 60.0 °C
2600 psi

@Temperature 140 °F
Cure cycle: 7 days @ RT , with Aced Etched 6061-T6 Aluminum
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste
Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some..
Shear Strength 17.9 MPa

@Temperature 100 °C
2600 psi

@Temperature 212 °F
Lap Shear, Cured at 250°C for 60 min at 30 psi MMM-A-132 and MIL-A-25463.
Hexcel® Redux® 382H (0.06 psf) Film Adhesive
Redux 382H is a 250°F curing modified epoxy film adhesive available in both supported and unsupported versions. Redux 382H is a versatile adhesive system suitable for bonding a wide variety of subs..
Shear Strength 17.9 MPa

@Temperature 93.3 °C
2600 psi

@Temperature 200 °F
Lap Shear
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.06 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Shear Strength 17.9 MPa

@Temperature 65.0 °C,
Time 3600 sec
2600 psi

@Temperature 149 °F,
Time 1.00 hour
Lap, Alum to Alum
Atom Adhesives AA-BOND F110 Epoxy Adhesive
AA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. AA-BOND F110 is room temperature system an excellent choice for thin bond-line assembly and repair applications of prisms..