Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.65 MPa @Time 1.21e+6 sec |
240 psi @Time 336 hour |
Graphite Bismaleimide (BMI) composite IM7/5250-4 |
3M AC-350 Class C-1/2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Shear Strength | 1.65 MPa @Time 1.21e+6 sec |
240 psi @Time 336 hour |
Graphite Bismaleimide (BMI) composite IM7/5250-4 |
3M AC-350 Class C-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Shear Strength | 1.65 MPa @Time 1.21e+6 sec |
240 psi @Time 336 hour |
Graphite Bismaleimide (BMI) composite IM7/5250-4 |
3M AC-350 Class C-8(24) Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Shear Strength | 1.65 MPa @Temperature -40.0 °C |
240 psi @Temperature -40.0 °F |
Overlap, Nylon |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 1.65 MPa @Temperature -40.0 °C |
240 psi @Temperature -40.0 °F |
Overlap, Nylon |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 1.65 MPa @Temperature -40.0 °C |
240 psi @Temperature -40.0 °F |
Overlap, Nylon |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |