Mechanical Properties Metric English Comments
Shear Strength 24.8 MPa

@Temperature 23.9 °C
3600 psi

@Temperature 75.0 °F
Cure cycle: 7 days @ RT (+7 days water soak) , with Aced Etched 6061-T6 Aluminum
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste
Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some..
Shear Strength 24.8 MPa

@Temperature 204 °C
3600 psi

@Temperature 400 °F
Tensile Lap Shear; Aluminum No Primer; ASTM D1002
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Shear Strength 24.8 MPa

@Temperature 21.1 °C
3600 psi

@Temperature 70.0 °F
Tensile Lap Shear; Titanium with HP655P; ASTM D1002
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Shear Strength 24.8 MPa

@Temperature 121 °C
3600 psi

@Temperature 250 °F
Overlap
3M Scotch-Weld™ 1469 One-Part Epoxy Adhesives and Metal Primer
High Temperature strength and Low ViscosityInformation provided by 3M
Shear Strength 24.8 MPa

@Temperature 71.0 °C
3600 psi

@Temperature 160 °F
with Scotch-Weld EW-5000, 14 days at 71°C and 95% RH; ASTM D1002-10
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive
3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion..
Shear Strength 24.8 MPa

@Temperature 82.0 °C
3600 psi

@Temperature 180 °F
Adhered: 50 MIL (17-7 Stainless Steel), Adhesive AF-126 (0.06 wt)
3M Scotch-Weld™ 3901 Metal Primer
3M™ Scotch-Weld™ Metal Primer 3901 is a primer for 3M™ Scotch-Weld™ film and liquid adhesives in those applications where it is desired to obtain improved metal and glass adhesion or improved re..