Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.138 MPa @Temperature 66.0 °C |
20.0 psi @Temperature 151 °F |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Shear Strength | 0.138 MPa @Temperature 66.0 °C |
20.0 psi @Temperature 151 °F |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Shear Strength | 0.138 MPa @Temperature 175 °C |
20.0 psi @Temperature 347 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.138 MPa @Temperature 175 °C |
20.0 psi @Temperature 347 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.138 MPa @Temperature 66.0 °C |
20.0 psi @Temperature 151 °F |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Shear Strength | 0.138 MPa @Temperature 82.0 °C |
20.0 psi @Temperature 180 °F |
Overlap, Solvent Wiped Steel |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.138 MPa @Temperature 82.0 °C |
20.0 psi @Temperature 180 °F |
Overlap, Solvent Wiped Steel |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 0.138 MPa @Temperature 82.0 °C |
20.0 psi @Temperature 180 °F |
Overlap, Solvent Wiped Steel |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |