Polymer Property : Shear Strength = 19.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 17.0 - 19.0 MPa

@Temperature 22.0 °C,
Time 86400 sec
2470 - 2760 psi

@Temperature 71.6 °F,
Time 24.0 hour
ISO 10123; Compressive, Steel pins and collars
Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-GP is a fast curing, GREEN, high strength, general purpose, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highl..
Shear Strength 17.0 - 19.0 MPa

@Temperature 22.0 °C,
Time 86400 sec
2470 - 2760 psi

@Temperature 71.6 °F,
Time 24.0 hour
ISO 10123; Compressive, Steel pins and collars
Palm Labs Adhesives TURBO-LOCK SERIES 17-HT Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-HT is a fast curing, GREEN, high temperature, high strength, high viscosity, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical p..