Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 112 MPa @Temperature 23.0 °C |
16200 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |