Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.03 MPa @Temperature 121 °C |
149 psi @Temperature 250 °F |
ASTM D1002-64 |
3M Scotch-Weld™ 3532 B/A Brown Two-Part Urethane Adhesive 3532 B/A Brown
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 20-30 minutes handling stren.. |
|||
Shear Strength | 1.03 MPa @Temperature 121 °C |
149 psi @Temperature 250 °F |
ASTM D1002-64 |
3M Scotch-Weld™ 3535 B/A Off-white Two-Part Urethane Adhesive 3535 B/A Off-white
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling stren.. |
|||
Shear Strength | 1.03 MPa @Temperature 121 °C |
149 psi @Temperature 250 °F |
ASTM D1002-64 |
3M Scotch-Weld™ 3549 B/A Brown Two-Part Urethane Adhesive 3549 B/A Brown
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include long worklife adhesive, 2-4 hours handling stren.. |