Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.03 MPa @Temperature 121 °C |
149 psi @Temperature 250 °F |
ASTM D1002-64 |
3M Scotch-Weld™ 3532 B/A Brown Two-Part Urethane Adhesive 3532 B/A Brown
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 20-30 minutes handling stren.. |
|||
Shear Strength | 1.03 MPa @Temperature 121 °C |
149 psi @Temperature 250 °F |
ASTM D1002-64 |
3M Scotch-Weld™ 3535 B/A Off-white Two-Part Urethane Adhesive 3535 B/A Off-white
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling stren.. |
|||
Shear Strength | 1.03 MPa @Temperature 121 °C |
149 psi @Temperature 250 °F |
ASTM D1002-64 |
3M Scotch-Weld™ 3549 B/A Brown Two-Part Urethane Adhesive 3549 B/A Brown
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include long worklife adhesive, 2-4 hours handling stren.. |
|||
Shear Strength | 1.03 MPa @Temperature 66.0 °C |
150 psi @Temperature 151 °F |
1/8" Birch/High-Pressure Laminate, aged 6 mo |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Shear Strength | 1.03 MPa @Time 605000 sec |
150 psi @Time 168 hour |
Overlap, Maple |
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Shear Strength | 1.03 MPa @Temperature 66.0 °C |
150 psi @Temperature 151 °F |
1/8" Birch/High-Pressure Laminate, aged 6 mo |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |