Mechanical Properties Metric English Comments
Flexural Strength 350 MPa

@Temperature 120 °C
50800 psi

@Temperature 248 °F
ISO 178
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Flexural Strength 350 MPa

@Temperature 23.0 °C
50800 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber
Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal..
Flexural Strength 350 MPa

@Temperature 20.0 °C
50800 psi

@Temperature 68.0 °F
DIN EN 843-1
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Flexural Strength 350 MPa

@Temperature 1000 °C
50800 psi

@Temperature 1830 °F
DIN EN 820-1
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Flexural Strength 350 MPa

@Thickness >=1.50 mm
50800 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..
Flexural Strength 350 MPa

@Thickness >=20.0 mm
50800 psi

@Thickness >=0.787 in
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..
Flexural Strength 350 MPa

@Temperature 23.0 °C
50800 psi

@Temperature 73.4 °F
ASTM D790
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp..
Copyright © lookpolymers.com All Rights Reserved