Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 43500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 300 MPa

@Temperature -40.0 °C
43500 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.0%); ASTM-D790
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 300 MPa

@Temperature -40.0 °C
43500 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 1.75%); ASTM-D790
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 300 - 400 MPa

@Temperature 23.0 - 1500 °C
43500 - 58000 psi

@Temperature 73.4 - 2730 °F
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..
Flexural Strength 300 MPa

@Thickness >=1.50 mm
43500 psi

@Thickness >=0.0591 in
1hr/150°C/measured at 150°C; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Flexural Strength 300 MPa

@Treatment Temp. 150 °C,
Time 3600 sec
43500 psi

@Treatment Temp. 302 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Flexural Strength 300 MPa

@Thickness >=1.50 mm
43500 psi

@Thickness >=0.0591 in
1hr/150°C/measured at 150°C; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t..