Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 360 MPa @Thickness >=1.60 mm, Temperature 200 °C |
52200 psi @Thickness >=0.0630 in, Temperature 392 °F |
Perpendicular to laminations; EN 60893 |
HOS-Technik Homide 250 Bismaleimide Resin Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel.. |
|||
Flexural Strength | 360 MPa @Strain 3.00 % |
52200 psi @Strain 3.00 % |
ISO 178 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Strength | 360 MPa @Temperature -40.0 °C |
52200 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 360 MPa @Temperature -40.0 °C |
52200 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 360 MPa @Thickness >=1.50 mm |
52200 psi @Thickness >=0.0591 in |
1hr/2000°C/measured at 2000°C; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |