Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 350 MPa @Temperature 120 °C |
50800 psi @Temperature 248 °F |
ISO 178 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
Flexural Strength | 350 MPa @Temperature 23.0 °C |
50800 psi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Flexural Strength | 350 MPa @Temperature 20.0 °C |
50800 psi @Temperature 68.0 °F |
DIN EN 843-1 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Flexural Strength | 350 MPa @Temperature 1000 °C |
50800 psi @Temperature 1830 °F |
DIN EN 820-1 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Flexural Strength | 350 MPa @Thickness >=1.50 mm |
50800 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Flexural Strength | 350 MPa @Thickness >=20.0 mm |
50800 psi @Thickness >=0.787 in |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Flexural Strength | 350 MPa @Temperature 23.0 °C |
50800 psi @Temperature 73.4 °F |
ASTM D790 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |