Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 240 MPa @Strain 3.80 % |
34800 psi @Strain 3.80 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Flexural Strength | 240 MPa @Strain 5.00 % |
34800 psi @Strain 5.00 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 240 MPa @Strain 5.00 % |
34800 psi @Strain 5.00 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 240 MPa @Thickness >=50.0 mm |
34800 psi @Thickness >=1.97 in |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Flexural Strength | 240 MPa @Temperature -40.0 °C |
34800 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |