Mechanical Properties Metric English Comments
Flexural Strength 225 MPa

@Temperature 23.0 °C
32600 psi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..