Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 300 MPa @Temperature -40.0 °C |
43500 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.0%); ASTM-D790 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 300 MPa @Temperature -40.0 °C |
43500 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.75%); ASTM-D790 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 300 MPa @Temperature 23.0 °C |
43500 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 300 - 400 MPa @Temperature 23.0 - 1500 °C |
43500 - 58000 psi @Temperature 73.4 - 2730 °F |
|
UBE Tyrannohex® Heat Resistant Composite Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe.. |
|||
Flexural Strength | 300 MPa @Thickness >=1.50 mm |
43500 psi @Thickness >=0.0591 in |
1hr/150°C/measured at 150°C; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Flexural Strength | 300 MPa @Treatment Temp. 150 °C, Time 3600 sec |
43500 psi @Treatment Temp. 302 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Flexural Strength | 300 MPa @Thickness >=1.50 mm |
43500 psi @Thickness >=0.0591 in |
1hr/150°C/measured at 150°C; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |