Polymer Property : Flexural Strength = 3.17 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 3.17 MPa

@Strain 5.00 %
460 psi

@Strain 5.00 %
Density 10 pcf; ASTM C203
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..
Flexural Strength 3.17 MPa

@Strain 5.00 %
460 psi

@Strain 5.00 %
Density 10 pcf; ASTM C203
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin
Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai..