Polymer Property : Flexural Strength = 19900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 137 MPa

@Temperature 200 °C
19900 psi

@Temperature 392 °F
ISO 178
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree..
Flexural Strength 137 MPa

@Temperature 200 °C
19900 psi

@Temperature 392 °F
2; ISO 178
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber
Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional ..
Flexural Strength 137 MPa

@Temperature 23.0 °C
19900 psi

@Temperature 73.4 °F
ASTM D790
DuPont Performance Polymers VESPEL TP-8054 Polyimide
DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi..