Mechanical Properties Metric English Comments
Flexural Strength 120 MPa

@Temperature -40.0 °C
17400 psi

@Temperature -40.0 °F
ASTM D790
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Flexural Strength 120 MPa

@Temperature 175 °C
17400 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
Flexural Strength 120 MPa

@Temperature 175 °C
17400 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
Flexural Strength 120 MPa

@Temperature 275 °C
17400 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Flexural Strength 120 MPa

@Temperature 175 °C
17400 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
Flexural Strength 120 MPa

@Temperature 175 °C
17400 psi

@Temperature 347 °F
ISO 178
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Flexural Strength 120 MPa

@Strain 8.00 %
17400 psi

@Strain 8.00 %
Conditioned; ISO 178
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers
PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized
Flexural Strength 120 MPa

@Strain 4.80 %
17400 psi

@Strain 4.80 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
Flexural Strength 120 MPa

@Temperature 80.0 °C
17400 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 1.7%); ASTM-D790
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 120 MPa

@Temperature -40.0 °C
17400 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.5%); ASTM-D790
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 120 MPa

@Temperature -40.0 °C
17400 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 3.0%); ASTM-D790
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 120 MPa

@Thickness >=250 mm
17400 psi

@Thickness >=9.84 in
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..