Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 154 MPa @Temperature -40.0 °C |
22300 psi @Temperature -40.0 °F |
ASTM D790 |
BASF Ultramid® 8281 HS GP PA6 (Dry) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |