Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.827 MPa @Strain 5.00 % |
120 psi @Strain 5.00 % |
Density 3 pcf; ASTM C203 |
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
Flexural Strength | 0.827 MPa @Strain 5.00 % |
120 psi @Strain 5.00 % |
Density 3 pcf; ASTM C203 |
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |