Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 99.9 kN/m | 570 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
Tear Strength | 99.9 kN/m | 570 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Tear Strength | 99.9 kN/m | 570 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Tear Strength | 99.9 kN/m | 570 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Tear Strength | 99.9 kN/m | 570 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude.. |
|||
Tear Strength | 99.9 kN/m | 570 pli | ASTM D624 |
Huntsman IROGRAN® A 89 E 4372 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Tear Strength | 99.9 kN/m | 570 pli | ASTM D624 |
Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tear Strength | 99.9 kN/m | 570 pli | ASTM D624 |
Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |