Polymer Property : Tear Strength = 98.2 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 98.2 kN/m
560 pli
Die C; ASTM D624
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Tear Strength 98.2 kN/m
560 pli
ASTM D624
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Tear Strength 98.2 kN/m
560 pli
ASTM D624
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether
Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext..
Tear Strength 98.2 kN/m
560 pli
Injection molded parts; ASTM D624
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester
Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext..
Tear Strength 98.2 kN/m
560 pli
ASTM D624
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Tear Strength 98.2 kN/m
560 pli
ASTM D624
Buckeye Polymers BP Flex D0853 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..