Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 163 kN/m | 930 pli | without incision; ISO 34B |
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
Tear Strength | 163 kN/m | 930 pli | ISO 34 |
Chengdu Polyster H605B Thermoplastic Polyether-ester Elastomer (TPEE) Medium modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Good melt stability. CVJ boots, dust cover, bellows, jackets and .. |
|||
Tear Strength | 163 kN/m | 930 pli | Graves (initial), MD; ASTM D1004 |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Tear Strength | 163 kN/m | 930 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR5725 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |