Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 92.0 kN/m | 525 pli | ASTM D624 |
Teknor Apex Telcar® TL-1000-95 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 92.0 kN/m | 525 pli | Die C; ASTM D-624 |
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio.. |