Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 7.00 - 9.00 kN/m | 39.9 - 51.4 pli | ASTM D624 Form B |
Dow BETAMATE™ 7200 Polyurethane Prepolymer BETAMATE™ 7200 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Tear Strength | 7.00 - 9.00 kN/m | 39.9 - 51.4 pli | ASTM D624 Form B |
Dow BETAMATE™ 7201 Polyurethane Prepolymer BETAMATE™ 7201 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Tear Strength | 7.00 - 9.00 kN/m | 39.9 - 51.4 pli | ASTM D624 Form B |
Dow BETAMATE™ 7205 Polyurethane Prepolymer BETAMATE™ 7205 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |