Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 15.1 kN/m | 86.2 pli | ASTM D412 |
Multibase TPSiV™ 3340-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 15.1 kN/m | 86.2 pli | ASTM D412 |
Multibase TPSiV™ 3340-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |