Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 14.0 kN/m | 79.9 pli | ISO 34-1 |
PolyOne OnFlex™ S FR 25A-3S1830 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3786/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ASTM D624 |
ELASTO UK Dryflex® 600300S SEBS Based Material, Filled Qualities, 30A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | |
ACC MM282 Specialist Molding 2-Part Condensation Cure Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | |
ACC MM906 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tear Strength | 14.0 kN/m | 79.9 pli | ISO 34-B |
AlphaGary Evoprene™ G 966 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |