Polymer Property : Tear Strength = 76.6 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 13.4 kN/m
76.6 pli
ASTM D624
Noble Polymers Ecobarrierâ„¢ 2412 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..