Polymer Property : Tear Strength = 679 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 119 kN/m
679 pli
Die C; ISO 34-1B
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application..