Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 113 kN/m | 645 pli | ASTM D1004 |
Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Lowest Modulus, Nominal Shore D/15s 35. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Tear Strength | 113 kN/m | 645 pli | ASTM D624 |
Toyobo PELPRENE™ P55B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Tear Strength | 113 kN/m | 645 pli | ASTM D624 |
Toyobo PELPRENE™ P55U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |