Polymer Property : Tear Strength = 6.14 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength >= 6.14 kN/m
>= 35.0 pli
ASTM D624
Parker Chomerics CHO-SEAL® 2557 Non-Conductive Extruded Elastomer Specifications
Description: Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL or CHO-SIL conductive elastomers are extruded in parallel with ..
Tear Strength >= 6.14 kN/m
>= 35.0 pli
ASTM D624
Parker Chomerics CHO-SEAL® 6503 Conductive Elastomer
Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric..
Tear Strength 6.14 kN/m
35.0 pli
ASTM D624
Parker Chomerics Tecknit Consil®-A 897 Silver-Aluminum Filled Silicone Elastomer
Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff..
Tear Strength 6.14 kN/m
35.0 pli
ASTM D624
Parker Chomerics Tecknit Consil®-C 875 Silver-Copper Filled Silicone Elastomer
Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s..
Tear Strength 6.14 kN/m
35.0 pli
ASTM D624
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer
Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se..
Tear Strength 6.14 kN/m
35.0 pli
ASTM D624
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer
Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi..
Tear Strength 6.14 kN/m
35.0 pli
ASTM D624
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by ..
Tear Strength 6.14 - 56.1 kN/m
35.0 - 320 pli
Average value: 32.9 kN/m Grade Count:9
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Tear Strength 6.14 kN/m
35.0 pli
Die B
Shin-Etsu Silicones KE-2090-10A/B Self-adhesive LIMS Silicone
ShinEtsuKE209010 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity o..
Tear Strength 6.14 kN/m
35.0 pli
Die B
Shin-Etsu Silicones KE-2090-20A/B Self-adhesive LIMS Silicone
ShinEtsu KE209020 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity ..
Tear Strength 6.14 kN/m
35.0 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7012-1000 TPE
Product Description: StarMediflex P7012-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:So..
Tear Strength 6.14 kN/m
35.0 pli
Initial Tear Strength
Saint-Gobain CHR® M730 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Tear Strength 6.14 kN/m
35.0 pli
Cytec EN-13 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Tear Strength 6.14 kN/m
35.0 pli
Cytec EN-14 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Tear Strength >= 6.14 kN/m
>= 35.0 pli
ASTM D624
Parker Chomerics CHO-SEAL® 2532 Non-Conductive Extruded Elastomer Specifications
Description: Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL conductive elastomers are extruded in parallel with non-conduct..
Tear Strength 6.14 kN/m
35.0 pli
Initial Tear Strength; ASTM D624 Die C
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..