Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 103 kN/m | 590 pli | ASTM D624 |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Tear Strength | 103 kN/m | 590 pli | ASTM D624 |
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tear Strength | 103 kN/m | 590 pli | ASTM D624 |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Tear Strength | 103 kN/m | 590 pli | |
Dow Corning SILASTIC® LSR 9791-70 A&B KIT 70 Durometer, 2-part, 1 to 1 mix, translucent, molding grade, Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Tear Strength | 103 kN/m | 590 pli | ISO 34-1 |
Alliance Polymers Viprene™ P55D-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 103 kN/m | 590 pli | ISO 34-1 |
Alliance Polymers Viprene™ P55D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P55D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |