Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 59.5 kN/m | 340 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ TM0200-0085 Black Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tear Strength | 59.5 kN/m | 340 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL 0135-33 Styrene Butadiene Block Copolymer (SBC) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tear Strength | 59.5 kN/m | 340 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 59.5 kN/m | 340 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Plasthall 7050 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 59.5 kN/m | 340 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 350ºF Cure Temperature Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 59.5 kN/m | 340 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Plasthall 7050 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 59.5 kN/m | 340 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 350ºF Cure Temperature Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 59.5 kN/m | 340 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Hi-Sil 233 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 59.5 kN/m | 340 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Hi-Sil 233 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |