Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 550 kN/m | 3140 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 550 kN/m | 3140 pli | ASTM D624 |
GRECO ISOTHANE 3080AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tear Strength | 550 kN/m | 3140 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, MD; ASTM D1004 |
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, TD; ASTM D1004 |
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, MD; ASTM D1004 |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, TD; ASTM D1004 |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, MD; ASTM D1004 |
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, TD; ASTM D1004 |
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, MD; ASTM D1004 |
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Graves, TD; ASTM D1004 |
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |
|||
Tear Strength | 550 kN/m | 3140 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |