Polymer Property : Tear Strength = 525 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 92.0 kN/m
525 pli
ASTM D624
Teknor Apex Telcar® TL-1000-95 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tear Strength 92.0 kN/m
525 pli
Die C; ASTM D-624
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..